ChemicalBook >> CAS DataBase List >>Polyethylene Terephthalate

Polyethylene Terephthalate

CAS No.
25038-59-9
Chemical Name:
Polyethylene Terephthalate
Synonyms
POLY(ETHYLENE TEREPHTHALATE);Mylar;Melinex;Superfloc;Pegoterate;Ethylene terephthalate polymer;Polyethylene terephthalate film;Terephtahlic acid-ethylene glycol polyester;Polyethyleneglycolterephthalateresin(PETF-61-BR);Poly(oxy-1,2-ethanediyloxycarbonyl-1,4-phenylenecarbonyl)
CBNumber:
CB6493400
Molecular Formula:
C10H12O6
Molecular Weight:
228.19868
MDL Number:
MFCD00084422
MOL File:
25038-59-9.mol
Last updated:2023-09-19 17:22:06

Polyethylene Terephthalate Properties

Melting point 250-255 °C
Boiling point >170 °C(Press: 10 Torr)
Density 1.68 g/mL at 25 °C
storage temp. Room Temperature
form pellets
color black
Indirect Additives used in Food Contact Substances POLY(ETHYLENE TEREPHTHALATE)
FDA UNII POLYETHYLENE TEREPHTHALATE (INTRINSIC VISCOSITY 0.70-1.00) (645M2T7FHZ)
POLYETHYLENE TEREPHTHALATE (INTRINSIC VISCOSITY 0.60-0.70) (5YSH70HE6K)
PEGOTERATE (JHW12Q65DD)
POLYETHYLENE TEREPHTHALATE (INTRINSIC VISCOSITY 1.00-2.00) (KJ6GWA9DJ0)
POLYETHYLENE TEREPHTHALATE (INTRINSIC VISCOSITY 0.40-0.70) (Y78AJD3DED)
EPA Substance Registry System Poly(ethylene terephthalate) (25038-59-9)

SAFETY

Risk and Safety Statements

Hazard Codes  Xi
Risk Statements  36/37/38
Safety Statements  26-36
WGK Germany  3
RTECS  TR2725000
HS Code  3921905050

Polyethylene Terephthalate price More Price(4)

Manufacturer Product number Product description CAS number Packaging Price Updated Buy
Sigma-Aldrich 1546900 Poly(ethylene terephthalate) United States Pharmacopeia (USP) Reference Standard 25038-59-9 3strips $457 2024-03-01 Buy
Sigma-Aldrich 3DXCNT004 3DXNANO™ ESD CNT-PETG carbon nanotube reinforced polyethylene terephthalate glycol copolymer 3D printing filament black, diam. 2.85?mm 25038-59-9 1EA $106 2023-06-20 Buy
Sigma-Aldrich 429252 Poly(ethylene terephthalate) granular 25038-59-9 250g $111 2024-03-01 Buy
TRC P688530 PolyethyleneTerephthalate,(contains30%glassparticlesasreinforcer) 25038-59-9 50mg $75 2021-12-16 Buy
Product number Packaging Price Buy
1546900 3strips $457 Buy
3DXCNT004 1EA $106 Buy
429252 250g $111 Buy
P688530 50mg $75 Buy

Polyethylene Terephthalate Chemical Properties,Uses,Production

Description

Polyethylene terephthalate (PET) is a saturated thermoplastic polyester. The first PET fibers, DacronTM and TeryleneTM, were first developed by Whinfield and Dixon in England. The first DacronTM plant began production in 1953. PET is produced using direct polycondensation reaction with ethylene glycol and terephthalic acid.lt is widely used in synthetic fibers which simulate wool, cotton, or rayon. PET films MylarTM, MelinexTM) are biaxially oriented by cold stretching the extruded sheets in two directions. This increases the crystallinity and reduces the tendency to shrink when heated. PET films are used in capacitors,slot liners for motors,magnetic tape, x-ray film, photographic film, graphic art and drafting applications,and food packaging such as boil-in-bags.

Chemical Properties

Polyethylene terephthalate (PET) is a semi crystalline polymer possessing excellent chemical resistance, melt mobility and spinnability. The polymer is composed of repeating units as shown in the Figure 1. Each unit having a physical length of about 1.09 nm and a molecular weight of ~200. When it is produced from the reaction of terephthalic acid and ethylene glycol, it is capped on the left by H- and the right by –OH. Polymerization is thus accompanied by the production of water which is removed under elevated temperature and vacuum. Accordingly the presence of water in the molten state will rapidly depolymerize the structure so that thorough drying of the polymer prior to melt spinning of fibers is necessary.
Structure of Polyethylene terephthalate(PET)
The aromatic ring coupled with short aliphatic chain makes the polymer a stiff molecule as compared to other aliphatic polymers such as polyolefin or polyamide. The lack of segmental mobility in the polymer chains results in relatively high thermal stability. A textile grade polymer will have an average number of 100 repeat units per molecule so that the extended length of the typical polymer chain is about 100nm with a molecular weight about 20,000. Higher levels of polymerization produces higher strength fibers but the melt viscosity and stability of the melt to even tiny amounts of moisture causes hydrolytic degradation. The measurement of average degree of polymerization is done either by molten viscosity (by measuring the pressure drop through a calibrated orifice) or the viscosity of the diluted polymer in an appropriate solvent. The latter is measure of polymer chain length known as Intrinsic viscosity or IV and the value for a typical fiber grade polymer is 0.6 dl/g in 60/40 w/w mixture of phenol and tetrachloroethane solvent. The IV in the latter solvent is related to Mv (Viscosity average molecular weight) of the polymer by the Mark Howink equation (Equation 1).

Uses

The first stage to produce Polyethylene Terephthalate (PET) is the reaction of ethylene glycol with terephthalic acid or dimethyl terephthalate. After the initial reaction, two or three polymerization steps are then performed, depending on the required molecular weight. The chemical structure of PET is composed of repeated units. Each unit has a physical length of about 1.09 nm and a molecular weight of ~200. PET monomer consists from an aromatic ring coupled with a short aliphatic chain that makes PET a stiff molecule as compared to other aliphatic polymers such as polyolefin or polyamide. The lack of segmental mobility in the polymer chains results in relatively high thermal stability. A textile grade polymer will have an average number of 100 repeat units per molecule so that the extended length of the typical polymer chain is about 100 nm with a molecular weight of ~20,000. Higher levels of polymerization produce higher strength fibers but the melt viscosity and stability of the melt to even tiny amounts of moisture causes hydrolytic degradation.
Photo-degradation of PET occurs after exposure to near-ultraviolet light resulting in either chain scission by Norrish I and II reactions. Cross-linking also takes place and polymer becomes brittle, discolored, and with uneven surface. PET when exposed to UV light degrades rather rapidly leading to deterioration in physical and mechanical properties and develops intense yellow color. It has been suggested that the photo-oxidation of PET involves the formation of hydroperoxide species through oxidation of the CH2 groups adjacent to the ester linkages and the hydroperoxide species involving the formation of photoproducts through several pathways. The ester moieties in the terephthalate moiety as well as CH2 groups are strongly involved in the photo-degradation of PET. The vinyl ester ends also act as cross-linkers and gelling agents. They polymerize and the polymers thermally degrade to give yellow or brown polyenes that discolor the final polymer. The formation of highly conjugated species is catalyzed by carboxyl groups. The formation of colored species is followed by increase of more carboxyl terminated species. Hence, the product having higher carboxyl value is subject to more discoloration. Furthermore, as the carboxyl content increases, the thermo-oxidative stability decreases. The carboxyl end groups act as catalysts for further degradation.

Uses

Polyethylene terephthalate, commonly referred to by PET, is a member of the polyester family of polymers.The combination of properties like hardness and rigidity,dimensional stability, chemical resistance andlightweight, makes PET a flexible material widely used in several applications such as fibers, sheets, films,and beverage containers. Used in electrical parts including relay bases and lamp sockets, pump housings, gears, sprockets, chair arms, casters and furniture components.
Like other polyesters, PET is produced industrially by direct esterification of dicarboxylic acids with diols.Typical production processes are based on polymerization of ethylene glycol (MEG) with either purifiedterephthalic acid (PTA) or dimethyl terephthalate (DMT) in the presence of a metal catalyst.

Definition

ChEBI: Polyethylene terephthalate is a macromolecule composed of repeating ethylene terephthalate units. It is used in synthetic fibers; beverage, food and other liquid containers; thermoforming applications; and engineering resins often in combination with glass fiber.

Preparation

Poly(ethylene terephthalate) is prepared by the reaction of either terephthalic acid or dimethyl terephthalate with ethylene glycol, and its repeating unit has the general structure
structure of Poly(ethylene terephthalate)
The resin has the ability to be oriented by a drawing process and crystallized to yield a high-strength product.

General Description

Made using premium Eastman PETG + Multi-wall Carbon Nanotubes (CNTs). 3DXNano? CNT enchanced compounds are used in critical applications that require electrostatic discharge(ESD) protection and a high level of cleanliness. Manufatuered with consistency in mind-3DXTech uses a proprietary formulation of virgin Eastman PETG (Polyethylene Terephtalate Glycol Copolymer) resin; multi-wall carbon nanotubes; and process/dispersion modifiers in order to give you the best possible printing experience.

Benefits of PETG include:

  • Superior Chemical Resistance vs. ABS
  • Amorphous: Low and near isotropic shrinkage
  • Low moisture absorption: 3x lower vs. ABS
  • Very low odor emitted during printing
  • Superior ductility vs. ABS
  • Wide processing range: 230 - 270 °C

Benefits of CNTs include:

  • Consistent surface resistivity
  • low additive loading rates
  • Improved retention of impact & elongation
  • Low particulate contamination
  • Minimal contribution to outgassing and ionic contamination

Synthesis

The synthesis of PET begins with the esterification of either terephthalic acid or dimethyl terephthalate with ethylene glycol, yielding bis(hydroxyethyl)terephthalate (BHET). The BHET is then polymerized up to about 30 repeat units (Awaja and Pavel 2005). Next, to achieve a degree of polymerization (DP) of about 100 repeat units, polycondensation is performed at temperatures > 270°C and pressures > 50 Pa (Ravindranath and Mashelkar 1986). To produce bottle-grade PET, the DP must be > 150 repeat units, which is typically accomplished via solidstate polymerization, a process that requires temperatures > 200°C, pressures > 100 Pa, and incubation times of at least 15 hr (Al-Ghatta et al. 1997).
It is becoming increasingly common for manufacturers to market copolymers for purposes previously filled by homopolymer PET. Copolymer blends, such as polybutylene terephthalate/PET, have certain advantages over homopolymer PET with regard to mechanical properties and resistance to degradation (Grossetête et al. 2000; GuerricaEchevarría and Eguiazábal 2009). In the United States, a clear plastic bottle may be made with copolymers and still be legally marketed as PET, according to applicable federal regulations [e.g., 21 CFR §177.1630 (U.S. Food and Drug Administration 2009).

Polyethylene Terephthalate Preparation Products And Raw materials

Global( 143)Suppliers
Supplier Tel Email Country ProdList Advantage
PT CHEM GROUP LIMITED
+86-85511178 +86-85511178 peter68@ptchemgroup.com China 35453 58
Hebei Yanxi Chemical Co., Ltd.
+8617531190177 peter@yan-xi.com China 5993 58
Henan Bao Enluo International TradeCo.,LTD
+86-17331933971 +86-17331933971 deasea125996@gmail.com China 2503 58
Henan Tianfu Chemical Co.,Ltd.
+86-0371-55170693 +86-19937530512 info@tianfuchem.com China 21691 55
career henan chemical co
+86-0371-86658258 sales@coreychem.com China 29914 58
Hubei Jusheng Technology Co.,Ltd.
18871490254 linda@hubeijusheng.com CHINA 28180 58
Hubei xin bonus chemical co. LTD
86-13657291602 linda@hubeijusheng.com CHINA 22968 58
Chongqing Chemdad Co., Ltd
+86-023-61398051 +8613650506873 sales@chemdad.com China 39916 58
Shaanxi Dideu Medichem Co. Ltd
+86-029-81138252 +86-18789408387 1057@dideu.com China 3586 58
Zhengzhou Alfa Chemical Co.,Ltd
+8618530059196 sale04@alfachem.cn China 12468 58

View Lastest Price from Polyethylene Terephthalate manufacturers

Image Update time Product Price Min. Order Purity Supply Ability Manufacturer
poly(ethylene terephthalate) macromolecule pictures 2023-09-19 poly(ethylene terephthalate) macromolecule
25038-59-9
US $50.00 / kg 1kg 0.99 10000 Hebei Yanxi Chemical Co., Ltd.
Poly(ethylene terephthalate) pictures 2023-07-22 Poly(ethylene terephthalate)
25038-59-9
US $100.00 / kg 1kg 99% 500t/month Henan Bao Enluo International TradeCo.,LTD
Polyethylene Terephthalate  pictures 2022-07-22 Polyethylene Terephthalate
25038-59-9
US $1.10 / g 1g 99.00% 100 Tons Min Dideu Industries Group Limited
arnitea arnitea-049000 arnitea200 arnitefp800 arniteg arniteg600 Cassappret sr cassappretsr lumirror38s Meliform Melinex O melinexo Mitsubishi kasei GF-PET 6010G15 Mylar A Mylar C Mylar C-25 Mylar hs Mylar T mylara mylarc mylarc-25 mylarhs mylart Nitron lavsan nitron(polyester) nitronlavsan Petra 130 Petra 130FR Petra 230 Petra 242 Poly(oxyethyleneoxyterephthaloyl) Polyestergranular polyethyleneterephthalatefilm RTP 1105FR Scotch par scotchpar Tenite PET 9902 terephtahlicacid-ethyleneglycolpolyester Terfan Tergal Terom Terphan Traytuf ultra-clea Traytuf ultra-clear Ultralen SP 3700 S Ultralen SP 3705 Valox 9215 VFR 3801 vfr3801 Vituf Estrofol B Estrofol Ow estrofolb estrofolow ethyleneterephthalatepolymer Fiber V fiberv Grilpet EV-30