Resists heat and corrosion, making it an ideal lining for refractory
furnaces.
製造方法
Hafnium (IV) oxide is prepared by calcination of the hydroxide, oxalate, oxychloride or sulfate at 600-1000 ℃. The crystallization of the oxide starts at 400 ℃.